R&D Magazine

Featured Headlines from the R&D Daily
Van Gogh’s hidden works are brought to life
Flexible, one-step assembly of nanoscale structures
Scientists spy an electron dance


Search R&D
 
Search Tips

SUBSCRIPTIONS

Magazine
   Digital
   Print
   Renew

The R&D Daily
   Recent Newsletters
   Subscribe
   Contact
   Advertise

Laboratory Design
   Newsletter Homepage
   Digital Edition
   Subscribe


FREE SUBSCRIPTIONS to R&D Magazine and Newsletters










Awards

R&D 100 Awards

Lab of the Year

Product Solutions

R&D e-Solutions

R&D Product Showcase


Materials Science/ Nanotechnology Feature

OLEDs could soon wave lifetime woes goodbye

April 23, 2008

Researchers have developed an improved organic light emitting diode (OLED) sealing process to reduce moisture intrusion and improve device lifetime.

OLEDs are promising for the next generation of displays and solid state lighting because they use less power and can be more efficiently manufactured than current technology. However, the intrusion of moisture into the displays can damage or destroy an OLED’s organic material.

“OLEDs have better color and flexibility and the capability of larger displays, but companies still need an inexpensive encapsulation method that can be used to mass produce organic electronics that don’t allow moisture in,” says Wusheng Tong, a senior research scientist at the Georgia Tech Research Institute (GTRI).

Manufacturers now seal displays in an inert atmosphere or in a vacuum environment. They glue a glass lid on top of the display substrate with a powder inside the display to absorb moisture that diffuses through the glue. These seals are expensive and labor-intensive to assemble.

With funding from GTRI’s independent research and development program, Tong and his GTRI collaborators—senior research scientist Hisham Menkara and principal research scientist Brent Wagner—have replaced the glass enclosure with a thin-film barrier formed by a less expensive conventional deposition method.

“We chose a passivation coating process that could be performed at room temperature so that the organic material remained intact,” says Tong.

The researchers selected advanced ion-assisted deposition, which utilizes reactive ions to deposit a high-density, pinhole-free thin silicon oxynitride (SiON) film on the OLED surface.

“Ideally, the film should be as thin as possible, but if it’s too thin, a pinhole or other defect could appear and cause a problem,” explains Tong. “We found that a film of 50-200 nm thickness was perfect.”

During testing, the SiON-encapsulated OLEDs showed no sign of degradation after seven months in an open-air environment, while the OLEDs without the coating degraded completely in less than two weeks under the same conditions.

When Tong conducted accelerating aging tests in an environmental chamber that maintained a temperature of 50°C and 50% relative humidity, the OLEDs encapsulated with SiON films showed little degradation for at least two weeks. The OLEDs without encapsulation, however, decomposed immediately.

“We’ve demonstrated that this deposition process improves the lifetime of the OLEDs by blocking the intrusion of moisture, so now we’re hoping to work with industry partners to develop a mass production process for our encapsulation technique,” adds Tong.

SOURCE: Georgia Institute of Technology


E-mail for more information

E-mail to a colleague

Printer friendly format


   Show Archived Articles











Events Calendar

More Events



























Bioscience Technology Chromatography Techniques Drug Discovery & Development Laboratory Equipment Pharmaceutical Processing R&D Scientific Computing
Advantage Business Media © Copyright 2008 Advantage Business Media
Privacy Policy | Terms & Conditions | Advertise With Us